Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Seong-Jin Lee, Kyeong-Min Kim, Heeshin Kang, Seong-Moon Seo, Wonah Park, Eun-Joon Chun
J Weld Join. 2023;41(4):254-264.   Published online 2023 Aug 31     DOI: https://doi.org/10.5781/JWJ.2023.41.4.4
Citations to this article as recorded by Crossref logo
New findings on reduced solidification brittle temperature range in epitaxially grown CMSX-4 superalloy welds via varestraint testing
Min-Chang Shin, Eun-Joon Chun
Materials Today Communications.2025; 42: 111201.     CrossRef
Effect of Single Crystal Growth and Solidification Grain Boundaries on Weld Solidification Cracking Behavior of CMSX-4 Superalloy
Kyeong-Min Kim, Ye-Seon Jeong, D.V. Kiran, Suk-Hwan Kwon, Seong-Moon Seo, Eun-Joon Chun
Korean Journal of Metals and Materials.2024; 62(1): 22.     CrossRef