Strategy of Suppressing the Solidification Cracking Susceptibility of 247LC Superalloy Weld Metals using Commercial Ni-Based Fillers
Eun-Joon Chun
J Weld Join. 2023;41(1):64-72. Published online 2023 Feb 21 DOI: https://doi.org/10.5781/JWJ.2023.41.1.7
|
Citations to this article as recorded by
Applicability of Hf-Free 247LC as a Filler Metal for Hot Crack-Free 247LC Superalloy Welds Assisted by Varestraint Testing
Seong-Jin Lee, Eun-Joon Chun
Materials.2025; 18(6): 1284. CrossRef Effect of local carbide formation behavior on repair weld liquation cracking susceptibility for long-term-serviced 247LC superalloy
Hye-Eun Jeong, Seong-Moon Seo, Eun-Joon Chun
Journal of Materials Research and Technology.2024; 28: 110. CrossRef Effect of Single Crystal Growth and Solidification Grain Boundaries on Weld Solidification Cracking Behavior of CMSX-4 Superalloy
Kyeong-Min Kim, Ye-Seon Jeong, D.V. Kiran, Suk-Hwan Kwon, Seong-Moon Seo, Eun-Joon Chun
Korean Journal of Metals and Materials.2024; 62(1): 22. CrossRef Effects of Hf and carbides formation behavior on the weld solidification cracking susceptibility of 247LC superalloy
Seong-Jin Lee, Seong-Moon Seo, Eun-Joon Chun
Materials Chemistry and Physics.2024; 316: 129147. CrossRef A Primary Study on the Applicability of Gel-Type Filler Materials to Root Pass Welds of the Thick Plate
Young-Min Kim, Sangwoo Nam, Insung Hwang, Jason Cheon, Byeong-Jin Kim
Journal of Welding and Joining.2024; 42(5): 487. CrossRef Solidification Crack Free Welding Strategy via Ultra High Precision Laser Scanning at a Single Grain of Directionally Solidified and Single Crystal Superalloys
Seong-Jin Lee, Kyeong-Min Kim, Heeshin Kang, Seong-Moon Seo, Wonah Park, Eun-Joon Chun
Journal of Welding and Joining.2023; 41(4): 254. CrossRef
|