Welding Deformation Characteristics and Mitigation Method of Hub Flange
Ji-Sun Roh, Chang-Woo Park, Jung-Goo Park
J Weld Join. 2022;40(5):393-400. Published online 2022 Oct 21 DOI: https://doi.org/10.5781/JWJ.2022.40.5.4
|
Citations to this article as recorded by
Features of Mechanical Properties and Residual Stress Distribution in Butt Joint of HSB690-SM355 Dissimilar Steel
Tae-Hwan Um, Kyong-Ho Chang, Jae-Yik Lee, Nizam Khan Sazid, Mikihito Hirohata
International Journal of Steel Structures.2024; 24(3): 565. CrossRef
|