Microstructure and Wear Characteristics of Multilayer Laser-Cladded Hypereutectic Al-Si Alloys
Hyoung-Keun Lee
J Weld Join. 2022;40(1):48-53. Published online 2022 Feb 9 DOI: https://doi.org/10.5781/JWJ.2022.40.1.6
|
Citations to this article as recorded by
Wear and Microstructural Characteristics of Colmonoy-4 and Stellite-6 Additive Layer Deposits on En19 Steel by Laser Cladding
Venu Kumar Sarila, Harisivasri Phanindra Koneru, Venkateswar Reddy Pathapalli, Muralimohan Cheepu, Venkata Charan Kantumuchu
Transactions of the Indian Institute of Metals.2023; 76(2): 457. CrossRef
|