Weldability Evaluation of GMAW and GTAW for Al-6.7 wt.% Mg Alloy
Taehoon Kang, Jiyoung YU, Young-Min Kim, Insung Hwang, Seung Hwan Lee, Dong-Yoon Kim
J Weld Join. 2021;39(5):471-479.   Published online 2021 Oct 25     DOI: https://doi.org/10.5781/JWJ.2021.39.5.2
Citations to this article as recorded by Crossref logo
Improving the Metal Inert Gas Welding Efficiency and Microstructural Stability in the Butt and Lap Joints of Aluminum Automotive Components Using Sc- and Zr-Enhanced Filler Wires
Hansol Ko, Hye-Jin Kim, Dong-Yoon Kim, Jiyoung Yu
Metals.2024; 15(1): 1.     CrossRef
Machine Learning Approach for the Prediction of Defect Characteristics in Wire Arc Additive Manufacturing
Muralimohan Cheepu
Transactions of the Indian Institute of Metals.2023; 76(2): 447.     CrossRef
Effects of Laser and Tungsten Arc Welding Processes on the Thermal Softening and Mechanical Properties of Almag6 Aluminum Alloy
Yeonho Kwak, Taehoon Kang, Seung Hwan Lee, Minjung Kang
International Journal of Precision Engineering and.2023; 24(4): 531.     CrossRef
Prediction of Weld Tensile-Shear Strength using ANN Based on the Weld Shape in Aluminum Alloy GMAW
Dong-Yoon Kim, June Hyung Hwang, Gwang-Gook Kim, Young-Min Kim, Jiyoung Yu, Junhong Park
Journal of Welding and Joining.2023; 41(1): 17.     CrossRef
Optimization of Welding Process Parameter for Gap Response in Aluminum GMAW Using Taguchi Method
Hyojun Choi, Taehoon Kang, Jiyoung Yu, Young-Min Kim, Seung Hwan Lee, Dong-Yoon Kim
Journal of Welding and Joining.2023; 41(1): 28.     CrossRef
Prediction Model for Tensile Shear Strength of Gas Metal Arc Weld using a Laser Vision Sensor
Changhoon Lee, Dong-Yoon Kim, Jason Cheon, Jiyoung Yu
Journal of Welding and Joining.2023; 41(5): 349.     CrossRef