Review on the Resistance Spot Weldability of Medium-Mn TRIP steel
Gitae Park, Sangho Uhm, Changhee Lee
J Weld Join. 2021;39(3):239-245. Published online 2021 Jun 28 DOI: https://doi.org/10.5781/JWJ.2021.39.3.2
|
Citations to this article as recorded by
Liquid Metal Embrittlement Cracking in Uncoated Transformation-Induced Plasticity Steel during Consecutive Resistance Spot Welding
Jae Won Kim, Sunusi Marwana Manladan, Kaisar Mahmud, Woosung Jin, Tejaswin Krishna, Changwook Ji, Dae-Geun Nam, Yeong-Do Park
Metals.2023; 13(11): 1826. CrossRef Metallurgical Factors Affecting the Tensile Properties of Weld Heat-Affected Zone in Medium Mn Transformation-Induced Plasticity Steel
Gitae Park
Journal of Welding and Joining.2022; 40(4): 329. CrossRef
|