Effect of Microstructure on Low-Temperature Impact Toughness of Multi-Pass Weld Metal of 1 GPa Class High Strength Steel
Yongjoon Kang, Changhee Lee
J Weld Join. 2021;39(3):233-238. Published online 2021 Jun 24 DOI: https://doi.org/10.5781/JWJ.2021.39.3.1
|
Citations to this article as recorded by
Alleviation of Hydrogen Embrittlement to Delay Effective Hydrogen Diffusion Against MA Constituent Formation Due to Mo Solutes for 420 MPa Grade Offshore Steels
Jimin Nam, Junghoon Lee, Hanji Park, Cheolho Park, Changhoon Lee, Junho Chung, Seung-gun Lee, Namhyun Kang
Metals and Materials International.2023; 29(6): 1625. CrossRef Prediction on cold crack sensitivity using hydrogen embrittlement index measured from in situ slow-strain-rate testing for multipass flux-cored arc weld metals of shipbuilding and offshore steels
Jaeseok Yoo, Hyoungjin An, Junghoon Lee, Kwang Hee Yun, Sourav Kr. Saha, Namhyun Kang
Materials Characterization.2023; 197: 112637. CrossRef Mo addition of high-strength seismic rebars subjected to Tempcore processes for tensile strength enhancement
Woonam Choi, Hyungsic Um, Hyangjun Yi, Namhyun Kang
Materials & Design.2022; 219: 110766. CrossRef Comprehensive Analysis of Cold-Cracking Ratio for Flux-Cored Arc Steel Welds Using Y- and y-Grooves
Hyunbin Nam, Jaeseok Yoo, Kwanghee Yun, Guo Xian, Hanji Park, Namkyu Kim, Sangwoo Song, Namhyun Kang