Determination of Optimal Weld Parameter for Joining Titanium Alloys by Gas Tungsten Arc Welding using Taguchi Method
Nazmul Huda, Jae Won Kim, Changwook Ji, Dae-Geun Nam, Yeong-Do Park
J Weld Join. 2021;39(1):81-88.   Published online 2021 Feb 4     DOI: https://doi.org/10.5781/JWJ.2021.39.1.10
Citations to this article as recorded by Crossref logo
Effect of heat input on microstructure and mechanical property of wire-arc additive manufactured Ti-6Al-4V alloy
Guo Xian, Jeong mok Oh, Junghoon Lee, Sang Myung Cho, Jong-Tak Yeom, Yoonsuk Choi, Namhyun Kang
Welding in the World.2022; 66(5): 847.     CrossRef
Effect of Welding Speed on Microstructure and Anisotropic Properties of Wire-Arc Additive-Manufactured Ti-6Al-4V alloy
Guo Xian, Jieun Yu, Muralimohan Cheepu, Sang Myung Cho, Namhyun Kang
Transactions of the Indian Institute of Metals.2022;[Epub]     CrossRef
Enhancing Tensile Properties of Wire-Arc Additively Manufactured Ti-6Al-4 V Deposits Via Cryogenic Vaporised Ar Shielding/Cooling
Guo Xian, Muralimohan Cheepu, Jieun Yu, Sang Myung Cho, Jong-Taek Yeom, Yoon Suk Choi, Namhyun Kang
Metals and Materials International.2022;[Epub]     CrossRef