Weld Shape Analysis using Central Composite Design in the Laser Welding of Aluminum Alloys
Donghyeok Choi, Joonghan Shin
Journal of Welding and Joining. 2020;38(5):502-507.   Published online 2020 Sep 16     DOI: https://doi.org/10.5781/JWJ.2020.38.5.10
Citations to this article as recorded by Crossref logo
A Study on the Correlation between Bead Geometry and Tensile Strength of Single Lap jointed Dissimilar Combinations through Regression Analysis
Jae Won Kim, Jae-Hwang Kim, Kwang-jin Lee, Sung-Wook Kang, Changwook Ji
Journal of Welding and Joining.2021; 39(2): 159.     CrossRef