Effect of Ar Plasma Treatment for Surface of Insert Metal on Property of TLP Bonding Joint for Power Module
Seungju Baek, Dong-Yurl Yu, Jun-Hyuk Son, Junghwan Bang, Jungsoo Kim, Min-Su Kim, Han-Bo-Ram Lee, Yong-Ho Ko
J Weld Join. 2020;38(4):366-373. Published online 2020 Aug 24 DOI: https://doi.org/10.5781/JWJ.2020.38.4.5
|
Citations to this article as recorded by
A Study on Aging Fracture Behavior of Sintered Joint by Bi-Modal Cu Paste
Junhyuk Son, Chang-Woo Lee, Dong-Yurl Yu, Dongjin Byun, Junghwan Bang
Journal of Welding and Joining.2022; 40(6): 540. CrossRef
|