A Study on the Effect of Plating Layer on the Corrosion Properties of Steel/Al Dissimilar Magnetic Pulse Weldments
Byoung-Hyun Yoon, Ji-Yeon Shim, Bong-Yong Kang
J Weld Join. 2020;38(3):305-310.   Published online 2020 Jun 1     DOI: https://doi.org/10.5781/JWJ.2020.38.3.11
Citations to this article as recorded by Crossref logo
Probing magnetic pulse welding of aluminium and steel sheets
Rishabh Shotri, Guillaume Racineux, Amitava De
Journal of Manufacturing Processes.2021; 72: 309.     CrossRef