Microstructure and Mechanical Properties of Friction-Welded Alloy 718 and SNCRW Stainless Steel After Post-Weld Heat-Treatment
Jeoung Han Kim, Nam-Yong Kim, Yu Sik Kong, Nho Kwang Park
J Weld Join. 2019;37(4):313-317. Published online 2019 Aug 30 DOI: https://doi.org/10.5781/JWJ.2019.37.4.4
|
Citations to this article as recorded by
Evaluation of the mechanical properties of Inconel 718 to SCM 440 dissimilar friction welding through real-time monitoring of the acoustic emission system
Yu Sik Kong, Muralimohan Cheepu, Jin-Kyung Lee
Proceedings of the Institution of Mechanical Engin.2021; 235(5): 1181. CrossRef
|