Characteristic of Welding Rotational Deformation in Laser Welding of Thin Steel Sheet
Jeong-Ung Park, Jong-Bong Lee, Gyubaek An, Sang-min Kim, Hwan-woong Seo
J Weld Join. 2018;36(6):1-7. Published online 2018 Dec 3 DOI: https://doi.org/10.5781/JWJ.2018.36.6.1
|
Citations to this article as recorded by
Analysis of Laser Heat Distribution in Al-Cu Welding
Hae Woon Choi
Journal of the Korean Society of Manufacturing Pro.2021; 20(2): 1. CrossRef Laser Welding of ASTM A553-1 (9% Nickel Steel) (PART I: Penetration Shape by Bead on Plate)
Jaewoong Kim, Jisun Kim, Sungwook Kang, Kwangsan Chun
Metals.2020; 10(4): 484. CrossRef Optimization of Optics Design for 3D Laser Scanner
Hae Woon Choi
Journal of the Korean Society of Manufacturing Pro.2020; 19(6): 96. CrossRef Laser Welding of ASTM A553-1 (9% Nickel Steel) (PART II: Comparison of Mechanical Properties with FCAW)
Jaewoong Kim, Jisun Kim
Metals.2020; 10(8): 999. CrossRef
|