A Study of Characteristics on the Dissimilar Metals (Alloy steel : A387 Gr. 91 - Carbon Steel : A516 Gr. 70) Welds Made with FCA Multiple Layer Welding: Part 2
Tae Woo Shin, Jun Hyeok Hyun, Jin Hyun Koh
J Weld Join. 2017;35(3):68-74. Published online 2017 Jun 30 DOI: https://doi.org/10.5781/JWJ.2017.35.3.10
|
Citations to this article as recorded by
Effect of Low Transformation Temperature Welding Consumable on Microstructure, Mechanical Properties and Residual Stress in Welded Joint of A516 Carbon Steel
Sungki Choi, Junsang Lee, Jae-Yik Lee, Seung-Kyun Kang, Young-Cheon Kim, Seung-Joon Lee, Dongil Kwon
Korean Journal of Metals and Materials.2021; 59(8): 524. CrossRef
|