Effect of Tool Plunge Depth on Weldability of Dissimilar Al5083-O/DP590 Friction Spot Joint
Su-Ok Jeong, Han-Sur Bang, Hee-Seon Bang
J Weld Join. 2016;34(3):17-22.   Published online 2016 Jun 30     DOI: https://doi.org/10.5781/JWJ.2016.34.3.17
Citations to this article as recorded by Crossref logo
Effects of processing parameters on the friction stir spot joining of Al5083-O aluminum alloy to DP590 steel
Back-Sub Sung, Hee-Seon Bang, Su-Ok Jeong, Woo-Seong Choi, Yong-Hyuk Kwon, Han-Sur Bang
Metals and Materials International.2017; 23(3): 562.     CrossRef