Effect of Restraint Stress on the Precipitation Behavior and Thermal Fatigue Properties of Simulated Weld Heat Affected Zone in Ferritic Stainless Steel
Kyutae Han, Yongjoon Kang, Sangchul Lee, Seunggab Hong, Hongchul Jeong, Changhee Lee
J Weld Join. 2015;33(6):6-12. Published online 2015 Dec 31 DOI: https://doi.org/10.5781/JWJ.2015.33.6.6
|
Citations to this article as recorded by
Effect of Ni-based Fillers on Corrosion Resistance of Heat Affected Zone of Super Austenitic Stainless Steel (UNS S31254) Welded by GTAW
Jin Sung Park, Dong Min Cho, Seung Gab Hong, Tae Ho Yun, Sung Jin Kim
Korean Journal of Metals and Materials.2023; 61(6): 404. CrossRef
|