Optimization of arc brazing process parameters for exhaust system parts using box-behnken design of experiment
Yong Kim, Pyeong-Won Park, Ki-Young Park, Jin-Chul Ryu
Journal of Welding and Joining. 2015;33(2):23-31.   Published online 2015 Apr 30     DOI: https://doi.org/10.5781/JWJ.2015.33.2.23
Citations to this article as recorded by Crossref logo
Evaluation of Structural Design Enhancement and Sensitivity of Automatic Ocean Salt Collector According to Design of Experiments
Chang Yong Song, Dong-Jun Lee, Jin Sun Lee, Eun Mi Kim, Bo-Youp Choi
Journal of Ocean Engineering and Technology.2020; 34(4): 253.     CrossRef
Effect of Various Factors on the Brazed Joint Properties in Al Brazing Technology
Ashutosh Sharma, Seung Hyun Lee, Hyung Oh Ban, Young Sik Shin, Jae-Pil Jung
Journal of Welding and Joining.2016; 34(2): 30.     CrossRef