Property Evaluation of Kinetic Sprayed Al-Ni Composite Coatings
GyeongJun Byun, JaeIck Kim, Changhee Lee, SeeJo Kim, Seong Lee
J Weld Join. 2014;32(5):502-509.   Published online 2014 Oct 30     DOI: https://doi.org/10.5781/JWJ.2014.32.5.72
Citations to this article as recorded by Crossref logo
Kinetic Spraying Deposition of Reactive-Enhanced Al-Ni Composite for Shaped Charge Liner Applications
Gyeongjun Byun, Jaeick Kim, Changhee Lee, See Jo Kim, Seong Lee
Journal of Thermal Spray Technology.2016; 25(3): 483.     CrossRef