A Study on Characteristics of Dissimilar Welds between Super Duplex Stainless Steel UNS S32750 and Carbon Steel A516-70 with FCAW
In-June Moon, Bok-Su Jang, Se-Cheol Kim, Jin-Hyun Koh
J Weld Join. 2014;32(4):364-371. Published online 2014 Aug 30 DOI: https://doi.org/10.5781/JWJ.2014.32.4.26
|
Citations to this article as recorded by
Microstructure and mechanical integrity relationship of PDC weld joints involving dissimilar marine grade alloys
Devendranath Ramkumar K., Nikam Pravin Pranav, Bhargav Sai, Arun D., Sam Vadakken Christin
Journal of Manufacturing Processes.2020; 50: 111. CrossRef A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW
Jun Hyeok Hyun, Tae Woo Shin, Sang Ho Kim, Jin Hyun Koh
Journal of Welding and Joining.2017; 35(4): 74. CrossRef
|