Effect of Preheat Temperature on Diffusible Hydrogen Content in Weld Metal Deposited using Flux Cored Wire
Dong Yoon Kim, In Sung Hwang, Dong Cheol Kim, Moon Jin Kang
J Weld Join. 2014;32(2):144-147. Published online 2014 May 14 DOI: https://doi.org/10.5781/JWJ.2014.32.2.18
|
Citations to this article as recorded by
Addition of cerium and yttrium to ferritic steel weld metal to improve hydrogen trapping efficiency
Sung Jin Kim, Kang Mook Ryu, Min-suk Oh
International Journal of Minerals, Metallurgy, and.2017; 24(4): 415. CrossRef A Numerical Study of the Residual Hydrogen Concentration in the Weld Metal
Jinsun Yoo, Yunsok Ha, Rajesh S.R.
Journal of Welding and Joining.2016; 34(6): 42. CrossRef A Review of Corrosion and Hydrogen Diffusion Behaviors of High Strength Pipe Steel in Sour Environment
Sung Jin Kim, Kyoo Young Kim
Journal of Welding and Joining.2014; 32(5): 13. CrossRef
|