Technical reports
Evaluation of Property and Reliability of Sn3.5Ag and Sn0.7Cu Pb-free Solder Joint by Complex Vibration for Application of Automobile Electric Module
Young-Ho Ko, Jung-Hwan Bang, Jeong-Han Kim, Chang-Woo Lee
J Weld Join. 2013;31(1):6-10.   Published online June 4, 2013
Recent Study of Overlay Welding on Welding methods
Ho-Cheon Yoo
J Weld Join. 2013;31(1):11-20.   Published online June 4, 2013
Special Issues
High Current Arc Welding Technology of Aluminum Alloy
Young-Bae Choi, Mun-Jin Kang, Dong-Cheol Kim, In-Sung Hwang
J Weld Join. 2013;31(1):21-25.   Published online June 4, 2013
Technology on Arc Welding Machine of Aluminum by Digital Control
Chang-Je LEE, Yu-Chan KIM, Jong-Do KIM
J Weld Join. 2013;31(1):26-32.   Published online June 4, 2013
Shielding Gases for Welding Aluminum
Douglas Steyer, Baesoo Jun
J Weld Join. 2013;31(1):38-42.   Published online June 4, 2013
Research Papers
Analysis of Microstructure for Resistance Spot Welded TRIP Steels using Atomic Force Microscope
Chul Young Choi, ChangWook Ji, Dae-Geun Nam, Jaeho Jang, Soon Kook Kim, Yeong-Do Park
J Weld Join. 2013;31(1):43-50.   Published online June 5, 2013
Evaluation of the Stress Occurring Phenomenon for Cold-Rolled Carbon Steel During a Laser Welding Process
Chulku Lee, Wooram Lee
J Weld Join. 2013;31(1):51-57.   Published online June 5, 2013
Microstructure and Tensile Strength Property of Arc Brazed DP steel using Cu-Sn Insert Metal
Wook-Je Cho, Young-Ho Cho, Jung-Gil Yun, Chung-Yun Kang
J Weld Join. 2013;31(1):58-64.   Published online June 5, 2013
Process Parameter Effect on Deformation of a V-groove Thin Plate for FCAW and EGW
Juho Han, Jaeseung Jeon, Chulsung Park, Chongin Oh, Jinoh Yun, Jeongsoo Lee
J Weld Join. 2013;31(1):65-70.   Published online June 5, 2013

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI