Heat treatment Technology of Electric Resistance Welding
Changhee Lee
J Weld Join. 2007;25(3):1-2.   Published online July 19, 2007
PDFPDF    
Effect of Welding Heat Input on Diffusible Hydrogen Content
Jae-Hak Kim, JunSeok Seo, HeeJin Kim, Hoi-Soo Ryoo
J Weld Join. 2007;25(3):3-5.   Published online July 19, 2007
PDFPDF    
Surface Microstructure Control via Friction Stir Process
Yong-Jai Kwon
J Weld Join. 2007;25(3):6-11.   Published online July 19, 2007
PDFPDF    
Fabrication Technique of Ultrafine Grained High-Strength Metallic Materials by Accumulative Roll-Bonding Process
Seong-Hee Lee, Sang-Shik Kim, Seung-Zeon Han, Cha-Yong Lim
J Weld Join. 2007;25(3):12-17.   Published online July 19, 2007
PDFPDF    
Characteristics of CW Nd:YAG Laser Lap Welds of Nickel Coated S45C Steel
Young-Tae Yoo, Ho-Jun Shin
J Weld Join. 2007;25(3):18-27.   Published online July 19, 2007
PDFPDF    
Effects of Amorphous Phase Fraction on the Scratch Response of NiTiZrSiSn Bulk Meatllic Glass in the Kinetic Spraying Process
Sanghoon Yoon, Sooki Kim, Changhee Lee
J Weld Join. 2007;25(3):28-36.   Published online July 19, 2007
PDFPDF    
Effect of Thermal Energy of In-Flight Particles on Impacting Behavior for NiTiZrSiSn Bulk Metallic Glass during Kinetic Spraying
Sanghoon Yoon, Sooki Kim, Changhee Lee
J Weld Join. 2007;25(3):37-44.   Published online July 19, 2007
PDFPDF    
Flow Characteristics and Filling Time Estimation for Underfill Process
Hyung-Sub Sim, Seong-Hyuk Lee, Jong-Min Kim, Young-Eui Shin
J Weld Join. 2007;25(3):45-50.   Published online July 19, 2007
PDFPDF    
Intermetallic Compounds Behavior at Laser Overlay Interface of Aluminum and Fe-based Powder
Namhyun Kang, Yeon-Gon Yoo, Chang-Woo Lee, Jeong-Han Kim
J Weld Join. 2007;25(3):51-56.   Published online July 19, 2007
PDFPDF    
Electrochemical Migration Characteristics of Sn-3.0Ag-0.5Cu Solder Alloy in NaBr and NaF Solutions
Ja-Young Jung, Eun-Jung Jang, Young-Ran Yoo et al.
J Weld Join. 2007;25(3):57-63.   Published online July 19, 2007
PDFPDF    
Dissolution Phenomenon of the Base Metal during TLP Bonding Using the Modified Base Metal Powder and Ni Base Filler Metal Powder
Woo-young Song, Chang-ho Ye, Chung-yun Kang
J Weld Join. 2007;25(3):64-71.   Published online July 19, 2007
PDFPDF    
Characterization of Microstructure of WC-6.5%Co Cladding Layer by Electric Resistance Welding
Jinwoo Lee, Junbin Ko, YoungHo Lee
J Weld Join. 2007;25(3):72-77.   Published online July 19, 2007
PDFPDF    
국제 용접ㆍ접합학술대회 (IWJC-Korea 2007)
편집부
J Weld Join. 2007;25(3):92-95.   Published online July 19, 2007
PDFPDF    
학회소식
편집부
J Weld Join. 2007;25(3):96-107.   Published online July 19, 2007
PDFPDF    
회원사동정
편집부
J Weld Join. 2007;25(3):108-115.   Published online July 19, 2007
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI