1 The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   
Yool Byun, Sangwon Lee, Chanhee Park, Jongtaek Yeom, Namhyun Kang, JaeKeun Hong
Journal of Welding and Joining:1-5.  Publication Date (Web): August 14, 2017   Cited by 4
                  PDF Links
 
6 Recent Advances in Friction-stir Welding Process and Microstructural Investigation of Friction Stir Welded Pure Titanium   
Jae-Deuk Kim, Eun-Geun Jin, Siva Prasad Murugan, Yeong-Do Park
Journal of Welding and Joining:6-15.  Publication Date (Web): August 25, 2017   Cited by 4
                  PDF Links
 
16 Research Trend of Laser Welding and Weldability of High Speed Dissimilar Laser Lap Welding for Titanium   
Su-Jin Lee, Eunjoon Chun, Jeong SUH
Journal of Welding and Joining:16-22.  Publication Date (Web): August 14, 2017
                  PDF Links
 
23 Trend of DED type Additive Manufacturing Technology for Titanium   
Sungwook Kim, Chang-Keun Chun
Journal of Welding and Joining:23-28.  Publication Date (Web): August 25, 2017   Cited by 4
                  PDF Links
 
29 Manufacturing Process and Market Trends of Titanium powder for 3D Printing   
JunHo Hwang
Journal of Welding and Joining:29-33.  Publication Date (Web): August 18, 2017   Cited by 1
                  PDF Links
 
34 Flame Braze between Aluminum Alloy 5A06 and Low Carbon Steel Q235   
Nian-chun LÜ, Yang LIU, Guo-dong Hao, Yun-tao WANG
Journal of Welding and Joining:34-40.  Publication Date (Web): July 20, 2017
                  PDF Links
 
41 A Study on the Influence of Various Welding Sequence Schemes on the Gain in Strength of Square Hollow Section Steel T-Joint   
Milad Moradi, Hartmut Pasternak
Journal of Welding and Joining:41-50.  Publication Date (Web): July 20, 2017   Cited by 3
                  PDF Links
 
51 Microstructure Evolution and Corrosion Behavior in the Welds of High Interstitial FeCrMnNC Austenitic Stainless Steels   
Joonoh Moon, Heon-Young Ha, Tae-Ho Lee
Journal of Welding and Joining:51-57.  Publication Date (Web): July 21, 2017   Cited by 1
                  PDF Links
 
58 Recent Studies of the Laser Cladding of High Entropy Alloys   
Sangwoo Nam, Cheolhee Kim, Young-Min Kim
Journal of Welding and Joining:58-66.  Publication Date (Web): July 19, 2017   Cited by 8
                  PDF Links
 
67 Fabrication of Al-11.2Si Components by Direct Laser Metal Deposition for Automotive Applications   
Amrinder Singh, Abhishek Ramakrishnan, Guru Dinda
Journal of Welding and Joining:67-73.  Publication Date (Web): July 20, 2017   Cited by 2
                  PDF Links
 
74 A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW   
Jun Hyeok Hyun, Tae Woo Shin, Sang Ho Kim, Jin Hyun Koh
Journal of Welding and Joining:74-81.  Publication Date (Web): July 19, 2017
                  PDF Links
 
82 In-situ Strain Measurement of Submerged Arc Welding Process Through Application of Electronic Speckle Pattern Interferometry   
Uwe Reisgen, Rahul Sharma
Journal of Welding and Joining:82-88.  Publication Date (Web): August 14, 2017   Cited by 1
                  PDF Links
 
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.           Developed in M2PI