Mechanical Bonding Properties of SAC-SB Mixed Solder Containing Sn-58Bi Eutectic Solder
Myeong Jin Jung, Yi Hyeon Ha, Jong-Moon Park, Seung-Hyeon Kang, Jong-Min Kim, Byung-Seung Yim
J Weld Join. 2025;43(2):128-133.   Published online April 30, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032326
Mechanical Bonding Properties of Solderable Anisotropic Polymer Composite containing Low-Melting-Point and High-Melting-Point Solder Fillers
Yi Hyeon Ha, Myeong Jin Jung, Jong-Moon Park, Sung Woo Choi, Jong-Min Kim, Byung-Seung Yim
J Weld Join. 2024;42(2):149-154.   Published online April 30, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI