Development and Evaluation of Stainless Steel-Base Flux-Cored Wires for 9% Nickel Steel (Editors’ Choice)
Tae-Uk Park, Young-Cheon Jeong, Hee-Dae Im, Chang-hyun Choi, Woong Kil
J Weld Join. 2022;40(5):367-376.   Published online September 29, 2022
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    
Tensile and Microstructural Behaviors of Austenitic Stainless Steel GTA Welds for Cryogenic Application
Woosung Yang, Woong Kil, Byungrok Moon, Hyunbin Nam, Namhyun Kang
J Weld Join. 2020;38(4):400-408.   Published online July 23, 2020
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S
Woong Kil, Myeong-jun Shin, Kook-soo Bang
J Weld Join. 2017;35(5):65-70.   Published online September 13, 2017
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    
2031785
The Latest Technology Development Trends of Flux Cored Wire
Hee-Dae Im, Chang-Hyun Choi, Jae-Heon Jung, Woong Kil
J Weld Join. 2016;34(6):1-10.   Published online December 29, 2016
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI