39 Prediction Model for the Microstructure and Properties in Weld Heat Affected Zone: Ⅲ. Prediction Model for the Austenite Grain Growth Considering the Influence of Initial Austenite Grain Size in Weld HAZ of Precipitates Free Low Alloyed Steel
Sang-Ho Uhm, Joon-Oh Moon, Hong-Chul Jeong, Jong-Bong Lee, Changhee Lee
Journal of Welding and Joining:39-49.  Publication Date (Web): October 16, 2006
PDF Links
 
77 [Research Papers] Prediction Model for the Microstructure and Properties in Weld Heat Affected Zone : Ⅱ. Prediction Model for the Austenitization Kinetics and Austenite Grain Size Considering the Effect of Ferrite Grain Size in Fe - C - Mn Steel
Jong-Geun Ryu, Joon-Oh Moon, Chang-Hee Lee, Sang-Ho Uhm, Jong-Bong Lee, Woong-Sung Chang
Journal of Welding and Joining:77-87.  Publication Date (Web): April 3, 2006
PDF Links
 
17 Prediction Model for the Microstructure and Properties in Weld Heat Affected Zone : Ⅰ. Trends in The Development of Model for the Prediction of Material Properties in the Weld HAZ
Joon-Oh Moon, Chang-Hee Lee
Journal of Welding and Joining:17-26.  Publication Date (Web): September 22, 2005
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI