Optimization of Direct Energy Deposition of 304L Stainless Steel through Laser Process Parameters
SeongSeon Shin, Sung-Min Kwon, ChiYen Kim, JongHoon Lee, JunHo Hwang, HyunDeok KIm
J Weld Join. 2021;39(2):182-188.   Published online April 7, 2021
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Effect of Laser Power Feedback Control on Mechanical Properties of Stainless Steel Part Built by Direct Energy Deposition
ChiYen Kim, JiSung Kim, Ho Lee et al.
J Weld Join. 2020;38(2):197-202.   Published online April 3, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI