A Study on the Characteristics of Inherent Strain for Predicting Thermal Deformation in Additive Manufacturing
Seok-Chul Yun, Chunbiao Wu, Si Mo Yeon, Kyunsuk Choi, Jae-Woong Kim
J Weld Join. 2025;43(3):300-306.   Published online June 30, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032313
A Study on Deformation due to Steel Constraint during Butt Welding and Line Heating of Thick-Plate in FLNG Topside Bearing Node
Dong-Hee Park, Jung-Goo Park, Jae-Myung Lee
J Weld Join. 2024;42(1):18-26.   Published online February 28, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Study on Deformation According to Steel Constraints During Thick-Plate Fillet Welding and Line Heating
Dong-Hee Park, Jung-Goo Park, Chang-Woo Park et al.
J Weld Join. 2023;41(6):508-518.   Published online December 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032239
Secondary Thermal Deformation Characteristics of Stiffened Plate Exposed to Fire
Jeong-Hwan Kim, Seung-Su Yu, Myung-Su Yi, Jung-Kwan Seo
J Weld Join. 2022;40(5):385-392.   Published online October 14, 2022
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
MIG Welding Optimization of Muffler Manufacture by Microstructural Change and Thermal Deformation Analysis
Seung Ho Lee, Eok Soo Kim, Jin-Young Park, Jun Choi
J Weld Join. 2017;35(5):29-37.   Published online September 27, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI