A Experiment Study on Selection the Optimal Condition for GMA Root-pass Welding in Overhead and Vertical Position
Ji-Sun Kim, In-Ju Kim, Ill-Soo Kim
J Weld Join. 2012;30(6):42-48.   Published online December 23, 2012
PDFPDF    
An Experimental Study on Root-pass Welding of Open Gap by GMA Welding Process in Pipeline
Ji-Sun Kim, Ill-Soo Kim, Chang-Eun Park, Hyun-Ho Na, Ji-Hye Lee, Seong-Myeong Jung
J Weld Join. 2011;29(3):64-69.   Published online July 7, 2011
PDFPDF    
Selection of Optimal Welding Condition in Root-pass Welding of V-groove Butt Joint
Seok-chul Yun, Jae-Woong Kim
J Weld Join. 2009;27(1):95-101.   Published online March 12, 2009
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI