2032386
Influence of Longitudinal Laser Beam Oscillation on Hot Cracking and Stress Distribution in Laser-Welded Aluminum
Sanghoon Kang, Jason Cheon, Minjung Kang
J Weld Join. 2025;43(1):70-78.   Published online February 28, 2025
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032354
Research on the Optimization of Oscillation for the Joint Quality of Laser Welded Joints in Automobile Seat Frames
JiYoung Shin, HyeonJe Kim, JaeYong Jang, HyeongJong Kim, Yeong-Do Park
J Weld Join. 2024;42(5):445-457.   Published online October 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032282
A Variance Analysis on the Porosity Distribution of Laser Welded A365 Casting with a Dual Beam Laser Under Various Oscillation Conditions
Hyeonhee Kim, Yong Hoon Jang, Minjung Kang
J Weld Join. 2023;41(4):275-281.   Published online August 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Recent Trends about Modulation Technology of the Laser Beam Welding
Yong Kim, Cheolhee Kim
J Weld Join. 2018;36(4):47-57.   Published online August 31, 2018
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
Development of Twin Torch Compound Metal Arc Welding Process to Form for Wide Hardfacing Bead of Wearplate
Sang-Myung Cho, Sung-Deok Kim, Kyu-Min Hwang
J Weld Join. 2008;26(2):50-54.   Published online June 18, 2008
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI