Understanding the Effects of Surface Finish on Diffusion Bonding of AZ31 Alloys
Matthew Criado, Abhijit Roy, John Ohodnicki et al.
J Weld Join. 2023;41(5):317-326.   Published online October 31, 2023
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032180
Resistance Spot Weldability of Aluminum Alloy with 6 wt.% Magnesium
Mingyu Kim, Sehyeon Kim, Insung Hwang et al.
J Weld Join. 2021;39(5):480-488.   Published online October 27, 2021
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032065
A Review on Welding of Dissimilar Metals in Car Body Manufacturing
Md. Abdul Karim, Yeong-Do Park
J Weld Join. 2020;38(1):8-23.   Published online February 19, 2020
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2032036
A Study for the Characteristics of Laser Welding on Over-lap Joint of Thin Magnesium Alloy Sheet
Mokyoung Lee, Jaej Kim
J Weld Join. 2019;37(4):293-298.   Published online August 29, 2019
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031750
Optimizing the Friction Stir Spot Welding Parameters to Attain Maximum Strength in Al/Mg Dissimilar Joints
Manickam Sundaram, Balasubramanian Visvalingam
J Weld Join. 2016;34(3):23-30.   Published online June 30, 2016
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031591
Plasma Electrolytic Oxidation in Surface Modification of Metals for Electronics
Mukesh Kumar Sharma, Youngjoo Jang, Jongmin Kim, Hyungtae Kim, Jae Pil Jung
J Weld Join. 2014;32(3):241-247.   Published online June 30, 2014
PDFPDF    
The Weldability of the Dissimilar Magnesium Alloy Welded by Fiber Laser
Jong-Do Kim, Young-Sik Kim, Mook-Keun Song, Jung-Han Lee
J Weld Join. 2013;31(2):63-68.   Published online June 5, 2013
PDFPDF    
A Study on the Weldability of Magnesium Alloy by Laser Heat Source (Ⅰ) ; Comparison on Laser Weldability of AZ31B-H24 and AZ31B-O
Jung-Han Lee, Jong-Do Kim, Mun-Yong Lee
J Weld Join. 2012;30(5):70-75.   Published online November 30, 2012
PDFPDF    
A Study on Weld Defect and Their Alternatives during Lap Welding of AZ31B Magnesium Alloy by Pulsed Nd: YAG Laser
Jong-Do Kim, Jung-Han Lee, Young-Sik Kim
J Weld Join. 2011;29(3):82-88.   Published online July 7, 2011
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2026 by The Korean Welding and Joining Society.

Developed in M2PI