Advanced Search  
 JWJ Search

441 A Study on the Effect of Overlap Rate on Laser Beam Cleaning Characteristics while Cleaning Paint Using a Low Power Pulsed Laser(Ⅱ) - Analysis of Laser Cleaned Surface Characteristics for Various Pulse Overlap Rates -   
Ji-Eon Kim, Moo-Keun Song, Jong-Myoung Lee, Jeong-Hun Hyun, Jong-Do Kim
Journal of Welding and Joining:441-447.  Publication Date (Web): October 17, 2019   Cited by 5
                  PDF Links
 
226 Experimental Investigation of Laser Cutting on Cement Composites   
Youngjin Seo, Sukhoon Pyo, Dongkyoung Lee
Journal of Welding and Joining:226-230.  Publication Date (Web): June 27, 2019   Cited by 1
                  PDF Links
 
1 The Effects of PWHT on Tensile Properties and Microstructures for Laser Welds of Ti-6Al-4V Alloys   
Yool Byun, Sangwon Lee, Chanhee Park, Jongtaek Yeom, Namhyun Kang, JaeKeun Hong
Journal of Welding and Joining:1-5.  Publication Date (Web): August 14, 2017   Cited by 4
                  PDF Links
 
69 The Characteristics of Continuous Waveshape Control for the Suppression of Defects in the Fiber Laser Welding of Pure Titanium Sheet (Ⅱ) - The Effect According to Control of Overlap Weld Length -   
Jong-Do Kim, Ji-Sung Kim
Journal of Welding and Joining:69-74.  Publication Date (Web): December 29, 2016
                  PDF Links
 
62 The Characteristics of Continuous Waveshape Control for the Suppression of Defects in the Fiber Laser Welding of Pure Titanium Sheet (Ⅰ) - The Effect According to Applying Slope Up & Down -   
Jong-Do Kim, Ji-Sung Kim
Journal of Welding and Joining:62-68.  Publication Date (Web): December 29, 2016
                  PDF Links
 
6 The Study for Improving the Weldability of Pure Titanium Sheet by Using Fiber Laser - The Effect of Shielding Gas Nozzle Variable -   
Jong-Do Kim, Ji-Sung Kim
Journal of Welding and Joining:6-12.  Publication Date (Web): October 30, 2016   Cited by 2
                  PDF Links
 
27 A Study on HAZ Softening Characteristics of Fiber Laser Weldment for High-Strength Steel   
Min-Ho Park, Ill-Soo Kim, Jong-Pyo Lee, Byeong-Ju Jin, Do-Hyeong Kim, In-Ju Kim, Ji-Sun Kim
Journal of Welding and Joining:27-35.  Publication Date (Web): December 31, 2015   Cited by 2
PDF Links
 
606 A Study on Correlationship between the Induced Plasma and Emission Signals for In-process Monitoring in Stainless Steel Welding of Fiber Laser (Ⅱ)
- Properties Changes of the Measured Signals in a Thick Plate Welding -
  
Chang-Je Lee, Jong-Do Kim
Journal of Welding and Joining:606-610.  Publication Date (Web): December 31, 2014   Cited by 1
PDF Links
 
600 A Study on Correlationship between the Induced Plasma and Emission Signals for In-process Monitoring in Stainless Steel Welding of Fiber Laser (Ⅰ)
- Properties Changes of the Measured Signals in a Thin Plate Welding -
  
Chang-Je Lee, Jong-Do Kim
Journal of Welding and Joining:600-605.  Publication Date (Web): December 31, 2014
PDF Links
 
592 A Study on the Characteristic of Weld Joint and Tensile Fracture of SUS304 and Cu High-Speed Dissimilar Lap Welds by Single Mode Fiber Laser   
Su-Jin Lee, Jong-Do Kim, Seiji Katayama
Journal of Welding and Joining:592-599.  Publication Date (Web): December 31, 2014   Cited by 1
PDF Links
 
437 The Effects of Welding Wires on the Weldabilities of API X-100 with Laser-Arc Hybrid Welidng   
Sungwook Kim, MOK-Young Lee
Journal of Welding and Joining:437-442.  Publication Date (Web): October 30, 2014
PDF Links
 
295 Mechanical Properties of Cu and Ni Dissimilar Welds by High Welding Speed Using Single-Mode Fiber Laser   
Su-Jin Lee, Jong-Do Kim
Journal of Welding and Joining:295-302.  Publication Date (Web): June 30, 2014   Cited by 1
PDF Links
 
28 Characteristics of Plasma Emission Signals in Fiber Laser Welding of API Steel (Ⅳ)
- Correlation of Keyhole's Periodic Motion and FFT Analysis Results -
  
Jong-Do Kim, Chang-Je Lee, Jeong Suh
Journal of Welding and Joining:28-33.  Publication Date (Web): August 31, 2013   Cited by 2
PDF Links
 
17 Fiber Laser Welding in the Car Body Shop
- Laser Seam Stepper versus Remote Laser Welding -
  
Berthold Kessler
Journal of Welding and Joining:17-22.  Publication Date (Web): August 31, 2013   Cited by 3
PDF Links
 
60 Characteristics of Plasma Emission Signals in Fiber Laser Welding of API Steel (Ⅲ)   
Chang-Je Lee, Jong-Do Kim, Yu-Chan Kim
Journal of Welding and Joining:60-65.  Publication Date (Web): June 30, 2013   Cited by 3
PDF Links
 
63 The Weldability of the Dissimilar Magnesium Alloy Welded by Fiber Laser   
Jong-Do Kim, Young-Sik Kim, Mook-Keun Song, Jung-Han Lee
Journal of Welding and Joining:63-68.  Publication Date (Web): June 5, 2013   Cited by 1
PDF Links
 
314 Characteristics of Plasma Emission Signals in Fiber Laser Welding of API Steel (Ⅱ) - The Relationship between Welding Conditions and Emission Signals -
Chang-Je LEE, Jong-Do KIM, Yu-Chan KIM
Journal of Welding and Joining:314-320.  Publication Date (Web): September 21, 2012   Cited by 4
PDF Links
 
51 Characteristics of Plasma Emission Signals in Fiber Laser Welding for API Steel (Ⅰ) - Variation of Signals by Measuring Conditions
Jong-Do KIM, Chang-Je LEE, Mok-Young LEE
Journal of Welding and Joining:51-57.  Publication Date (Web): January 10, 2011
PDF Links
 
72 Weld Quality Quantification through Chaotic Analysis
Jung-Ho Cho, Dave Farson, Cheolhee Kim
Journal of Welding and Joining:72-76.  Publication Date (Web): March 10, 2010
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI