A Study on the Effects of Offset and Welding Speed on Bead Shape and Welding Defects in the FCA Fillet Welding Process
Junsung Bae, Sang-Hyun Ahn, Gwang-Ho Jeong, Seonmin Kim, Dae-Won Cho, Seokyoung Ahn
J Weld Join. 2024;42(5):539-549.   Published online October 31, 2024
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
2031863
Recent Advances in Friction-stir Welding Process and Microstructural Investigation of Friction Stir Welded Pure Titanium
Jae-Deuk Kim, Eun-Geun Jin, Siva Prasad Murugan, Yeong-Do Park
J Weld Join. 2017;35(4):6-15.   Published online August 25, 2017
Full textFull text    PubreaderPubReader    ePubePub    PDFPDF    
A Study on Weld Defect and Their Alternatives during Lap Welding of AZ31B Magnesium Alloy by Pulsed Nd: YAG Laser
Jong-Do Kim, Jung-Han Lee, Young-Sik Kim
J Weld Join. 2011;29(3):82-88.   Published online July 7, 2011
PDFPDF    
Development of Multi-pass Welding Method for Lifting Lug by Robot Weaving
Young-Zoo Kim, Kang-Uk Kim, Suk-Hyoung Kim, Sung-Won Kang, Soo-Ho Kim
J Weld Join. 2007;25(5):44-52.   Published online January 28, 2008
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2025 by The Korean Welding and Joining Society.

Developed in M2PI