305 A Study on the Effect of Plating Layer on the Corrosion Properties of Steel/Al Dissimilar Magnetic Pulse Weldments   
Byoung-Hyun Yoon, Ji-Yeon Shim, Bong-Yong Kang
Journal of Welding and Joining:305-310.  Publication Date (Web): June 1, 2020   Cited by 1
                  PDF Links
 
278 Effect of the Holding Time during Solution Heat Treatment on Intergranular Corrosion of Unstabilized Austenitic Stainless Steels   
Eun-Jong Oh, Dong-Hwa Lee, Sung-Woo Cho, Yun-Il Choi, Ki-Woo Nam
Journal of Welding and Joining:278-288.  Publication Date (Web): June 2, 2020   Cited by 2
                  PDF Links
 
322 Effect of Carbon Content on Intergranular Corrosion of Welding Heat Affected Zone in 304 Stainless Steel   
Eun-Jong Oh, Jae-Hyung Lee, Sung-Woo Cho, Won-Geun Yi, Ki-Woo Nam
Journal of Welding and Joining:322-332.  Publication Date (Web): July 22, 2019   Cited by 2
                  PDF Links
 
61 Anticorrosion Performance of FCAW Cladding with Regard to the Influence of Heat Input   
Manas Kumar Saha, Ajit Mondal, Ritesh Hazra, Santanu Das
Journal of Welding and Joining:61-69.  Publication Date (Web): October 10, 2018   Cited by 3
                  PDF Links
 
78 A Study on the Electrochemical Corrosion Property of Sn-xSb Solder Alloy   
Junhyuk Son, Dong-Yurl Yu, Yong-Ho Ko, Junghwan Bang
Journal of Welding and Joining:78-82.  Publication Date (Web): June 19, 2018   Cited by 1
                  PDF Links
 
72 Corrosion Properties and Failure Behavior of Al/Fe Self-Piercing Rivet Joint   
Sanghoon Kang, Jin Young Yoon, Cheolhee Kim
Journal of Welding and Joining:72-77.  Publication Date (Web): June 25, 2018   Cited by 2
                  PDF Links
 
34 Study on the Corrosion Resistance of High Strength Bolt, Nut and Washer Set (S10T) Related to the Surface Treatment Conditions   
Youn O Choi, Jung Woo Han, Hyun Seon Hong, Han Gil Suk
Journal of Welding and Joining:34-39.  Publication Date (Web): March 8, 2018   Cited by 1
                  PDF Links
 
89 The Effect of PWHT on the Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW   
Jun-Hyeok Hyun, Tae-Woo Shin, Bok-Su Jang, Sang-Ho Kim, Jin-Hyun Koh
Journal of Welding and Joining:89-95.  Publication Date (Web): December 15, 2017   Cited by 1
                  PDF Links
 
1 Corrosion Assessment for Boron Steel Weldments Prepared by Overlap Welding and Successive Hot Press Forming Processes   
Minjung Kang, Cheolhee Kim
Journal of Welding and Joining:1-6.  Publication Date (Web): October 10, 2017   Cited by 2
                  PDF Links
 
74 A Study on Characteristics of Duplex Stainless Steel (ASTM A240 UNS S31803) Weld Metals made with FCAW   
Jun Hyeok Hyun, Tae Woo Shin, Sang Ho Kim, Jin Hyun Koh
Journal of Welding and Joining:74-81.  Publication Date (Web): July 19, 2017
                  PDF Links
 
51 Microstructure Evolution and Corrosion Behavior in the Welds of High Interstitial FeCrMnNC Austenitic Stainless Steels   
Joonoh Moon, Heon-Young Ha, Tae-Ho Lee
Journal of Welding and Joining:51-57.  Publication Date (Web): July 21, 2017   Cited by 1
                  PDF Links
 
21 Cu Corrosion Test Method for Lead-Free Solders   
Mi-Song Kim, Won Sik Hong, Chul Min Oh, Keun-Soo Kim
Journal of Welding and Joining:21-27.  Publication Date (Web): June 30, 2017
                  PDF Links
 
7 Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints   
Jeonga Kim, Yujin Park, Chul Min Oh, Won Sik Hong, Yong-Ho Ko, Sungdo Ahn, Namhyun Kang
Journal of Welding and Joining:7-14.  Publication Date (Web): June 30, 2017
                  PDF Links
 
13 Laser Peening Application for PWR Power Plants   
Jong-Do Kim, Yuji SANO
Journal of Welding and Joining:13-18.  Publication Date (Web): October 30, 2016   Cited by 1
                  PDF Links
 
37 A Study of Characteristics on the Dissimilar Metals (STS 316L - Carbon Steel: ASTM A516-70) Welds made with GTAW   
Se Cheol Kim, Tae Woo Shin, In Joon Moon, Bok Su Jang, Jin Hyun Koh
Journal of Welding and Joining:37-43.  Publication Date (Web): August 31, 2015   Cited by 1
PDF Links
 
1 Laser Peening Process and Its Application Technique   
Jong-Do Kim, Muneharu KUTSUNA, Yuji SANO
Journal of Welding and Joining:1-6.  Publication Date (Web): August 31, 2015
PDF Links
 
49 A study on Zn corrosion resistance of WC spray coating sealed with carbon nanotube suspensions   
Bong-Hun Kim, Bo-Young Lee
Journal of Welding and Joining:49-53.  Publication Date (Web): February 28, 2015
PDF Links
 
550 Prediction of Cr Content in the Martensitic-hardfaced Weldment Utilizing Dilution Rate Analytically Estimated   
Bong-Hun Kim, Chun-Hwan Kim
Journal of Welding and Joining:550-557.  Publication Date (Web): December 31, 2014
PDF Links
 
443 A Review of Corrosion and Hydrogen Diffusion Behaviors of High Strength Pipe Steel in Sour Environment   
Sung Jin Kim, Kyoo Young Kim
Journal of Welding and Joining:443-450.  Publication Date (Web): October 30, 2014   Cited by 7
PDF Links
 
431 Evaluation of HIC/SSCC Resistance for API-X70 Pipe Manufactured by JCO Bending Process and SA Welding   
Hoi-Soo Ryoo, Hee Jin Kim, Dong-Eon Lee
Journal of Welding and Joining:431-436.  Publication Date (Web): October 30, 2014   Cited by 1
PDF Links
 
393 Corrosion Assessment of Al/Fe Dissimilar Metal Joint   
Minjung Kang, Cheolhee Kim, Junki Kim, Dongcheol Kim, Jonghoon Kim
Journal of Welding and Joining:393-400.  Publication Date (Web): August 30, 2014   Cited by 5
PDF Links
 
364 A Study on Characteristics of Dissimilar Welds between Super Duplex Stainless Steel UNS S32750 and Carbon Steel A516-70 with FCAW   
In-June Moon, Bok-Su Jang, Se-Cheol Kim, Jin-Hyun Koh
Journal of Welding and Joining:364-371.  Publication Date (Web): August 30, 2014   Cited by 1
PDF Links
 
274 Effects of the Electroless Ni-P Thickness and Assembly Process on Solder Ball Joint Reliability   
Ji-Hye Lee, Seok-Hwan Huh, Gi-Ho Jung, Suk-Jin Ham
Journal of Welding and Joining:274-281.  Publication Date (Web): June 30, 2014   Cited by 2
PDF Links
 
20 Heat Treatment Effect on Pitting Corrosion of Super Duplex Stainless Steel UNS S32750 FCA Welds   
Bok-Su Jang, In-June Moon, Se-Cheol Kim, Jin-Hyun Koh
Journal of Welding and Joining:20-25.  Publication Date (Web): November 5, 2013   Cited by 2
PDF Links
 
21 Researches in Corrosion Resistance of Friction Stir Welded Aluminum alloys   
Byung-Wook Ahn, Don-Hyun Choi, Yun-Mo Yeon, Seung-Boo Jung
Journal of Welding and Joining:21-25.  Publication Date (Web): June 5, 2013
PDF Links
 
56 A Study on Machining Effects on Residual Stress at Dissimilar Metal Weld Region
Kyoung-soo Lee, Jeong-geun Lee, Seong-ho Lee, Chi-yong Park, Seung-geon Lee, Jai-hak Park
Journal of Welding and Joining:56-63.  Publication Date (Web): May 7, 2011
PDF Links
 
18 Effect of Welding Thermal Cycle on Microstructure and Pitting Corrosion Property of Multi-pass Weldment of Super-duplex Stainless Steel
Seong-Kil Nam, Se-Jin Park, Hye-Sung Na, Chung-Yun Kang
Journal of Welding and Joining:18-25.  Publication Date (Web): September 8, 2010
PDF Links
 
85 Study on the Effects of Flows on the Acceleration of the Grooving Corrosion in the ERW Pipe
Jae-Seong Kim, Yong Kim, Bo-Young Lee
Journal of Welding and Joining:85-91.  Publication Date (Web): September 24, 2008
PDF Links
 
57 Electrochemical Migration Characteristics of Sn-3.0Ag-0.5Cu Solder Alloy in NaBr and NaF Solutions
Ja-Young Jung, Eun-Jung Jang, Young-Ran Yoo, Shin-Bok Lee, Young-Sik Kim, Young-Chang Joo, Tai-Joo Chung, Kyu-Hwan Lee, Young-Bae Park
Journal of Welding and Joining:57-63.  Publication Date (Web): July 19, 2007
PDF Links
 
1 |
e-submission
endonote style file
JWJ
vol: Issue: Page:
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society.           Developed in M2PI