Chul Min Oh 5 Articles
Effects of High Temperature-moisture on Corrosion and Mechanical Properties for Sn-system Solder Joints
Jeonga Kim, Yujin Park, Chul Min Oh et al.
J Weld Join. 2017;35(3):7-14.   Published online June 30, 2017
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    
Cu Corrosion Test Method for Lead-Free Solders
Mi-Song Kim, Won Sik Hong, Chul Min Oh, Keun-Soo Kim
J Weld Join. 2017;35(3):21-27.   Published online June 30, 2017
Full textFull text    PubreaderPubReader    ePubePub    CrossRef-TDMCrossref - TDM    PDFPDF    
Validation of sequence test method of Pb-free solder joint for automotive electronics
A Young Kim, Chul Min Oh, Won Sik Hong
J Weld Join. 2015;33(3):25-31.   Published online June 30, 2015
PDFPDF    
2031506
Degradation Behavior of Solder Joint and Implementation Technology for Lead-free Automotive Electronics
Won Sik Hong, Chul Min Oh
J Weld Join. 2013;31(3):22-30.   Published online June 30, 2013
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI