2031702
The Effect of Nano Functionalized Block Copolymer Addition on the Joint Strength of Structural Epoxy Adhesive for Car Body Assembly
Hye-rim Lee, So-jeong Lee, Chang-young Lim, Jong-dock Seo, Mok-soon Kim, Jun-ki Kim
J Weld Join. 2015;33(4):44-49.   Published online August 31, 2015
PDFPDF    
2031538
The Effect of Zirconate Addition on the Joint Properties of Epoxy Adhesive for Car Body Assembly
Eun-taek Jeung, Hye-rim Lee, So-jeong Lee et al.
J Weld Join. 2013;31(5):71-76.   Published online November 5, 2013
PDFPDF    

Journal of
Welding and
Joining

Print ISSN: 2466-2232
Online ISSN: 2466-2100

Register for e-submission  Register for e-submission
Register here to access the e-submission system of Journal of Welding and Joining for authors and reviewers.
Register for e-submission  Manuscript Submission
To submit a manuscript, please visit the Journal of Welding and Joining e-submission management system at https://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of Welding and Joining e-submission system.
For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Register for e-submission  Free archive
Anyone may access any past or current articles without logging in.


ABOUT
BROWSE ARTICLES
ARTICLE CATEGORY 
FOR CONTRIBUTORS
Editorial Office
#304, San-Jeong Building, 23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
Tel: +82-2-538-6511    Fax: +82-2-538-6510    E-mail: koweld@kwjs.or.kr                

Copyright © 2022 by The Korean Welding and Joining Society.

Developed in M2PI