doi:https://doi.org/10.5781/JWJ.2019.37.4.7    [Epub ahead of print]
A Study on the Bead Shape and Changing Material Properties Depending on the Welding Position in P-GMAW
Jin-Hyeong Park*, Sung-Hwan Kim*, Roh-Won Kim*, Hyeong-Soon Moon*, Myung-Hyun Kim**
*Precision Manufacturing & Control R&D Group, Korea Institute of Industrial Technology, Busan, 46742, Korea
**Dept. of Naval Architecture and Ocean Engineering, Pusan National University, Busan 46241, Korea
Correspondence: Hyeong-Soon Moon  Email: hsmoon@kitech.re.kr, kimm@pusan.ac.kr
Myung-Hyun Kim  Email: hsmoon@kitech.re.kr, kimm@pusan.ac.kr
Received May 19, 2019  Accepted June 25, 2019  Published online July 22, 2019
ABSTRACT
This study performed welding in different positions, in the flat, vertical down, overhead positions, using the P-GMAW process. Despite using the same amount of heat input, the welding characteristics varied depending on the welding position. The effect of gravity on the welding process determined the formation of the weld bead. The difference in molten pool behavior for various welding positions resulted in changes in the microstructure due to differences in cooling rates. To collect the welding parameters, the current and voltage signals were synchronized with a high speed camera using a DAQ system. To induce one droplet for one pulse of metal transfer, a shielding gas composite rate was used, 95%Ar+5%CO2. The results in the melting zone for different welding positions were compared, and the microstructure of the welded section related to molten pool behavior was analyzed.
Keywords: Welding position | Molten pool behavior | Cooling rate | Gravity
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
211
View
2
Download
Related articles
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Influence of the Welding Speeds and Changing the Tool Pin Profiles on the Friction Stir Welded AA5083-O Joints   2017 June;35(3)
A Study on Surface and Cross-section Properties Depending on the Process Parameters of Laser Depositions with Metal Powders (SUS316L and IN718)  2017 June;35(3)
A Study on the Optimal Welding Methods of Vertical Welding Positions in the Vehicle Body  2010 December;28(6)
A Study on the Mechanical Properties of MAG Weld on Ferritic Stainless Steel Sheets  2009 April;27(2)
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Influence of the Welding Speeds and Changing the Tool Pin Profiles on the Friction Stir Welded AA5083-O Joints   2017 June;35(3)
A Study on Surface and Cross-section Properties Depending on the Process Parameters of Laser Depositions with Metal Powders (SUS316L and IN718)  2017 June;35(3)
A Study on the Optimal Welding Methods of Vertical Welding Positions in the Vehicle Body  2010 December;28(6)
A Study on the Mechanical Properties of MAG Weld on Ferritic Stainless Steel Sheets  2009 April;27(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.