Advanced Search  
JWJ > Epub ahead of print
doi:https://doi.org/10.5781/JWJ.2020.38.1.6    [Epub ahead of print]
Review on Mitigation of Welding-Induced Distortion Based on FEM Analysis
Chunbiao Wu*, Jae-Woong Kim**
*Department of Mechanical Engineering, Graduate School of Yeungnam University, Gyeongsan, 38541, Korea
**School of Mechanical Engineering, Yeungnam University, Gyeongsan, 38541, Korea
Correspondence: Jae-Woong Kim  Email: jaekim@ynu.ac.kr
Received April 11, 2019  Accepted September 23, 2019  Published online January 20, 2020
ABSTRACT
Welding distortion is an unavoidable issue due to localized expansion and contraction during the heating and cooling cycles, and has a negative effect on the fabrication process. However, mitigating weld distortion to meet product requirements is a challenging task, because welding shrinkage can’t be prevented, only controlled. This paper provides a comprehensive literature review of various techniques to reduce and optimize the deformation induced by welding in the design stage and manufacturing process. Finite element numerical analysis methods are usually employed to predict welding distortion, and can cost less than actual experiments. The review of these approaches is useful to fully understand the main mechanisms used to mitigate weldinginduced distortion, and for choosing the most suitable method to minimize deformation based on realistic fabrication requirements.
Keywords: Welding distortion | Optimization | FEM analysis | Welding process | Welding sequence; Artificial intelligence | Mechanical and thermal balance control method
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
0
Crossref
54
View
0
Download
Related articles
Construction of Welding Information Infra System   2002 February;20(1)
Investigation on Metal Transfer in GMA Welding through Dimensional Analysis   1999 February;17(1)
A Study on the Mitigation of Welding Distortion of a Precision Component for Automobile Transmission  2012 August;30(4)
Construction of Welding Information Infra System   2002 February;20(1)
Investigation on Metal Transfer in GMA Welding through Dimensional Analysis   1999 February;17(1)
A Study on the Mitigation of Welding Distortion of a Precision Component for Automobile Transmission  2012 August;30(4)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.