Effect of Moisture Content of Air on Diffusible Hydrogen Content in GMAW Process
Jae-Hak Kim, Hee-Jin Kim, Jun-Seok Seo, Hoi-Soo Ryoo



Correspondence:   Published online January 28, 2008
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,013
View
0
Download
Related articles
Effects of Winding Position and Air Time on Diffusible Hydrogen Content in Weld Metal using Flux Cored Wire  2020 October;38(5)
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S  2017 October;35(5)
Influence of Surface Roughness of Tools on the Friction Stir Welding Process  2014 December;32(6)
Effect of Preheat Temperature on Diffusible Hydrogen Content in Weld Metal Deposited using Flux Cored Wire  2014 April;32(2)
Quantitative Analysis on the Effects of Welding Parameters on Diffusible Hydrogen Contents in Weld Metal Produced by FCAW Process  2010 April;28(2)
Effects of Winding Position and Air Time on Diffusible Hydrogen Content in Weld Metal using Flux Cored Wire  2020 October;38(5)
Effects of Fluoride in the Flux on Hydrogen Content in Weld Metal and Operating Behavior in FCAW-S  2017 October;35(5)
Influence of Surface Roughness of Tools on the Friction Stir Welding Process  2014 December;32(6)
Effect of Preheat Temperature on Diffusible Hydrogen Content in Weld Metal Deposited using Flux Cored Wire  2014 April;32(2)
Quantitative Analysis on the Effects of Welding Parameters on Diffusible Hydrogen Contents in Weld Metal Produced by FCAW Process  2010 April;28(2)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.