ABSTRACT
  Since the 1990"s, European shipbuilding industries introduced hybrid welding process in order to decrease thermal distortion of welded joints in passenger shipbuilding. In this study, we investigated effects of hybrid welding parameters on the toughness of weld metal using DH36 steel in order to obtain more sound welds in passenger shipbuilding. Type of leading process, joint gap distance and chemical composition of consumables were considerably correlated with the toughness of weld metal. Especially, the toughness was considerably increased with high-Ti containing consumables. In addition, hybrid welding speed increased by using plasma cut edges, the oxides layer of which increased absorption efficiency of laser beam.
Keywords: Hybrid welding;Toughness;Weld metal
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,041
View
0
Download
Related articles
Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding by using AISI 430 Stainless Steel Strip - Experimental Study  2017 October;35(5)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels  2017 February;35(1)
Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding   2017 February;35(1)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
Effects of Welding Parameters on the Overlay Welding Behaviors in Electroslag Cladding by using AISI 430 Stainless Steel Strip - Experimental Study  2017 October;35(5)
Laser Welding Characteristic of Dissimilar Metal for Aluminum to Steel  2017 September;35(5)
Effect of Post-Weld Heat Treatment on the Mechanical Properties and Microstructure of P-No. 1 Carbon Steels  2017 February;35(1)
Influence of Gas Metal Arc Welding Parameters on the Bead Properties in Automatic Cladding   2017 February;35(1)
Effects of Heat Inputs on the Mechanical Properties of FCA Weldment of YP 690MPa Grade Steels  2016 December;34(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.