Review on the International Joint Researches for Evaluation of Welding Residual Stresses
Jong-Sung Kim, June-Soo Park, Tae-Eun Jin


Correspondence:   Published online January 26, 2006
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
696
View
0
Download
Related articles
Development and Application of the Battelle Structural Stress Method for Fatigue Evaluation of Welded Automotive Structures  2012 April;30(2)
A Review on the International Effects for the Fatigue Strength Assessment of Welded Structures  2005 December;23(6)
Prediction Model for Relaxation of Welding Residual Stress under Fatigue Loads  2002 June;20(3)
Analysis on the Fatigue Crack Propagation of Weld Toe Crack through Residual Stress Field   2000 October;18(5)
Review of Fatigue Strength Evaluation on Weld Joints of Hull Structure   1994 September;12(3)
Development and Application of the Battelle Structural Stress Method for Fatigue Evaluation of Welded Automotive Structures  2012 April;30(2)
A Review on the International Effects for the Fatigue Strength Assessment of Welded Structures  2005 December;23(6)
Prediction Model for Relaxation of Welding Residual Stress under Fatigue Loads  2002 June;20(3)
Analysis on the Fatigue Crack Propagation of Weld Toe Crack through Residual Stress Field   2000 October;18(5)
Review of Fatigue Strength Evaluation on Weld Joints of Hull Structure   1994 September;12(3)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.