Advanced Search  
JWJ > Volume 22(6); 2004 > Article
Journal of KWJS 2004 December;22(6) :57-63.
Published online January 26, 2005.
A Study on the Fracture Toughness Characteristics of FCAW Weldment of Steel for Offshore Structures
Sung-Won Kang, Myung-Hyun Kim, Yong-Bin Kim, Yong-Taek Shin, Hae-Woo Lee




Correspondence:   Published online January 26, 2005
ABSTRACT
Fracture toughness is an important parameter in designing offshore structures to ensure resistance to fracture at various temperatures. in this study, a series of experiments is carried out to obtain fracture toughness values (CTOD) of API 2W Gr.50B, welded using FCAW(Flux Cored Arc Weld). In particular, a comparison of absorbed impact energy and CTOD values are made with respect to two different welding groove shapes; double- V-groove and double-bevel-groove. Charpy impact tests are performed for specimens sampled near the root gap, and CTOD tests are carried out for three point bending specimens having the notch at weld zone. While Charpy impact test result is determined to be a good qualitative measure of fracture toughness, no quantitative correspondence between impact absorbed energy and CTOD values was found. Based on the experiment, it is observed that double- V-groove welds give lower transition temperature than those of double-bevel-groove.
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
1,121
View
0
Download
Related articles
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Study on Metallurgical Characteristic of Weld Metal for Gray Cast Irons - Weld Microstructure and Crack Sensitivity -  2018 February;36(1)
A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control  2017 October;35(5)
A Study on HAZ Softening Characteristics of Fiber Laser Weldment for High-Strength Steel   2015 December;33(6)
Study on Diffusion Bonding Characteristics of Austenitic Stainless Steels  2018 October;36(5)
Study on the Fracture Toughness of FCA Weldment with the Yield Strength 420MPa Grade High Strength Steels for Offshore Structures Depending on the Welding Position  2018 April;36(2)
Study on Metallurgical Characteristic of Weld Metal for Gray Cast Irons - Weld Microstructure and Crack Sensitivity -  2018 February;36(1)
A Study of Characteristics of Vertical-up SMA Welding by Short Circuit Control  2017 October;35(5)
A Study on HAZ Softening Characteristics of Fiber Laser Weldment for High-Strength Steel   2015 December;33(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.