Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 High Speed Welding Present and Future in Shipbuilding Assembly Stage

Journal of KWJS 2004;22(6):14-18.
Published online January 26, 2005.
[특집 : 고속용융용접기술 동향] 선박조립분야에 있어 고속용접 현황 및 전망
, ,
 
High Speed Welding Present and Future in Shipbuilding Assembly Stage
Tae-Won Jang, Jong-Hyun Moon, Dong-Ryeol Yoon