A Study on the Quality Estimation of Resistance Spot Welding Using Hidden Markov Model
김경일, 최재성

Correspondence:   Published online December 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
931
View
0
Download
Related articles
A Study on the Algorithm for Determining Back Bead Generation in GMA Welding Using Deep Learning  2018 April;36(2)
Strength Estimation Model of Resistance Spot Welding of 1.2GPa Grade Ultra High Strength TRIP Steel for Car Body Applications  2018 February;36(1)
Weld Quality Evaluation Method for the Resistance Spot Welds using X-ray Transmission Inspection  2014 December;32(6)
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode  2013 December;31(6)
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
A Study on the Algorithm for Determining Back Bead Generation in GMA Welding Using Deep Learning  2018 April;36(2)
Strength Estimation Model of Resistance Spot Welding of 1.2GPa Grade Ultra High Strength TRIP Steel for Car Body Applications  2018 February;36(1)
Weld Quality Evaluation Method for the Resistance Spot Welds using X-ray Transmission Inspection  2014 December;32(6)
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode  2013 December;31(6)
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.