Effect of Plaama Treatment on the Bond Strength of Sn-Pb Eutectic Solder Flip Chip
홍순민, 강순칙, 정재필


Correspondence:   Published online August 26, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
706
View
0
Download
Related articles
The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer  2019 June;37(3)
Effect of Fine Silica Filler Addition on the CTE and Void Behavior of Non-conductive Paste for CoB Flip Chip Bonding  2018 August;36(4)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
Effect of Curing Agent on the Curing Behavior and Joint Strength of Epoxy Adhesive  2011 August;29(4)
Effects of the Stand-off Distance on the Weld Strength in Magnetic Pulse Welding  2008 December;26(6)
The Effects of Heat Treatment Temperature on Wear Characteristics of Hyper-Eutectic Al-Si Alloy Laser Clad Layer  2019 June;37(3)
Effect of Fine Silica Filler Addition on the CTE and Void Behavior of Non-conductive Paste for CoB Flip Chip Bonding  2018 August;36(4)
Effects of Ni-P Bath on the Brittle Fracture of Sn-Ag-Cu Solder/ENEPIG Solder Joint   2017 June;35(3)
Effect of Curing Agent on the Curing Behavior and Joint Strength of Epoxy Adhesive  2011 August;29(4)
Effects of the Stand-off Distance on the Weld Strength in Magnetic Pulse Welding  2008 December;26(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.