Fatigue Life Prediction for Resistance Spot Weldment of Aluminum Alloy Sheet
장건익, 안병국, 김동건


Correspondence:   Published online April 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
623
View
0
Download
Related articles
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
Fatigue Life Prediction of Al 5083-O Weldment Considering the Overload Effect  2018 October;36(5)
The Resistance Spot Weldability of a Stainless Steel/Aluminium/Low Carbon Steel 3-Ply Clad Sheet  2018 February;36(1)
Design of Helical SPR for Joining Advanced High Strength Steel and Aluminum Alloy Sheets  2015 December;33(6)
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode  2013 December;31(6)
Effects of Electrode Face Radius and Force on Resistance Spot Weldability of Aluminium Alloy 6061  2018 December;36(6)
Fatigue Life Prediction of Al 5083-O Weldment Considering the Overload Effect  2018 October;36(5)
The Resistance Spot Weldability of a Stainless Steel/Aluminium/Low Carbon Steel 3-Ply Clad Sheet  2018 February;36(1)
Design of Helical SPR for Joining Advanced High Strength Steel and Aluminum Alloy Sheets  2015 December;33(6)
Electrode Life Test of Resistance Spot Welding on Mg Alloy Using Dome Type Electrode  2013 December;31(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
The Korea Science and Technology Building, New B/D, Room 503
Teheran-ro 7-gil, 22(635-4, Yeoksam-Dong), Gangnam-gu, Seoul 06130, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.