Parameter Design and Analysis for Aluminum Resistance Spot Welding
YongJoon Cho, Wei Li, S.Jack Hu


Correspondence:   Published online April 25, 2002
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
733
View
0
Download
Related articles
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
Dynamic Model for Electrode Expansion in Resistance Spot Welding Machines  2011 April;29(2)
Design of Erosion Resistant Overlay Welding Material  2010 June;28(3)
The Effects of Process Parameters on Sealing Quality for Ir-192 Radiation Source Capsule using Resistance Spot Welding  2009 February;27(1)
The Effect of Process Parameter on the Symmetry of Nugget in Micro-resistance Series Spot Welding   2001 December;19(6)
Monitoring of Resistance Spot Welding Processes  2012 February;30(1)
Dynamic Model for Electrode Expansion in Resistance Spot Welding Machines  2011 April;29(2)
Design of Erosion Resistant Overlay Welding Material  2010 June;28(3)
The Effects of Process Parameters on Sealing Quality for Ir-192 Radiation Source Capsule using Resistance Spot Welding  2009 February;27(1)
The Effect of Process Parameter on the Symmetry of Nugget in Micro-resistance Series Spot Welding   2001 December;19(6)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.