A Study on the Analysis of the Thermal Stress in Process of STS 304 TIG Welding
고준빈, 최원두, 이영호


Correspondence:   Published online December 25, 2001
TOOLS
PDF Links  PDF Links
Full text via DOI  Full text via DOI
Download Citation  Download Citation
CrossRef TDM  CrossRef TDM
  E-Mail
Share:      
METRICS
828
View
0
Download
Related articles
A Study on the Electrochemical Corrosion Property of Sn-xSb Solder Alloy  2018 June;36(3)
A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding  2018 February;36(1)
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on the Evaluation of Transverse Residual Stress at the Multi-pass FCA Butt Weldment using FEA  2010 August;28(4)
A Study on the Distortion of a Thin Plate Panel by Laser Welding  2007 February;25(1)
A Study on the Electrochemical Corrosion Property of Sn-xSb Solder Alloy  2018 June;36(3)
A Study on the Estimation of Weld Quality Using the Thermal Images During Arc Welding  2018 February;36(1)
A Study on the Welding Distortion Analysis According to Rib Height in Fillet Welding  2013 December;31(6)
A Study on the Evaluation of Transverse Residual Stress at the Multi-pass FCA Butt Weldment using FEA  2010 August;28(4)
A Study on the Distortion of a Thin Plate Panel by Laser Welding  2007 February;25(1)
e-sciencecentral
Register for e-submission
Register here to access the e-submission system of Journal of KWJS for authors and reviewers.
Manuscript Submission
To submit a manuscript, please visit the Journal of KWJS e-submission management system at http://submit.e-jwj.org, read the Instructions for Authors, and log into the Journal of KWJS e-submission system. For assistance with manuscript submission, please contact: koweld@kwjs.or.kr.
Free archive
Anyone may access any past or current articles without logging in.
Editorial Office
#304, San-Jeong Building,
23, Gukhoe-daero 66-gil, Yeongdeungpo-gu, Seoul 07237, Korea
TEL : +82-2-538-6511    FAX : +82-2-538-6510   E-mail: koweld@kwjs.or.kr
Browse Articles |  Current Issue |  For Authors and Reviewers |  About
Copyright© by The Korean Welding and Joining Society. All right reserved.