Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 A Materials-Based Approach to the Enhanced Fitness-For-Service Assessment for Welded Structures

Journal of KWJS 2001;19(5):26-32.
Published online October 25, 2001.
FAD를 이용한 용접구조물의 사용적합성 평가와 재료공학적 개선 방안
, , , ,
 
A Materials-Based Approach to the Enhanced Fitness-For-Service Assessment for Welded Structures
장재일, 이정석, 주장복, 권동일, 최열