Warning: fopen(/home/virtual/kwjs/journal/upload/ip_log/ip_log_2024-04.txt): failed to open stream: Permission denied in /home/virtual/lib/view_data.php on line 88 Warning: fwrite() expects parameter 1 to be resource, boolean given in /home/virtual/lib/view_data.php on line 89 Characteristics of Weld Quality Produced by the High Frequency Electric Resistance Welding Simulator

Journal of KWJS 2001;19(3):4-9.
Published online June 25, 2001.
ERW Simulator를 이용한 고주파 전기저항 용접부의 품질 특성
,
 
Characteristics of Weld Quality Produced by the High Frequency Electric Resistance Welding Simulator